1 / 5
| Mechanical Behavior | Standard Values |
|---|---|
| Density | 2.2 g/cm³ |
| Compressive Strength Key | 1100 MPa |
| Flexural Strength | 67 MPa |
| Poisson's Ratio | 0.14 ~ 0.17 |
| Young's Modulus | 72,000 MPa |
| Modulus of Rigidity | 31,000 MPa |
| Mohs Hardness | 5.5 ~ 6.5 |
| Transformation Point Key | 1280 °C |
| Softening Point | 1780 °C |
| Annealing Point | 1250 °C |
| Specific Heat (20 ~ 350 °C) | 670 J/kg·°C |
| Thermal Conductivity (20 °C) | 1.4 W/m·°C |
| Index of Refraction | 1.4585 |
| Low Thermal Expansion Coefficient Key | 5.5 × 10⁻⁷ cm/cm·°C |
| Thermal Processing Temperature | 1750 ~ 2050 °C |
| Short-Term Use Temperature | 1300 °C |
| Long-Term Use Temperature | 1100 °C |
| Material | Silicon Dioxide (Natural Quartz) |
| Color | Transparent or Colorless |
| Surface | No Air Bubble, No Line |
| Strain | 1270 °C Fused Quartz Glass Brick |
| PPM Grade | Controlled 10 / 20 / 100 PPM |
| Shape | Circle |
| Thickness | 2 MM – 20 MM |